Compression breaking load | Kg/cm2 | 917 |
Compression breaking load after freezing test | Kg/cm2 | 930 |
Bending Strength | Kg/cm2 | 144 |
Volumetric Weight | Kg/m3 | 2478 |
Water absorption at N.P. conditions | % | 3.07 |
Apparent porosity | % | 7.62 |
Thermal Linear expansion coefficient | X10-6perº C | 3.1 |
Abrasion Test | mm | 3.5 |
Impact test: minimum fall height | cm | 35-40 |
SiO2 | 0.06% |
AI2O3 | 0.23% |
Fe2O3 | 0.04% |
MnO | n.d. |
CaO | 55.76% |
MgO | 0.00% |
Na2O | 0.07% |
K2O | vest. |
TiO2 | 0.00 |
P.R | 43.82% |
CO2 | 43.76% |
District
Leiria
Municipality
Alcobaça